Fish pond anti-seepage Geomembrane
Classification :
keyword:
Geomembrane
PRODUCT DETAILS
Fish pond anti-seepage Geomembrane
| Name; geomembrane |
| Length; 1-6m |
| Thickness; 0.3 -2 mm |
| Material; HDPE, LDPE, PVC, LLDPE |
| Color; Black, white, blue, customized products can be supported according to customer needs |
Introduction
Geomembrane necessities are indispensable for making certain the notable and common standard ordinary overall performance of these materials. As a professional in the profits industry, I would like to emphasize the following necessities for geosynthetic membranes:
1. Materials: Geomembranes want to be made of exceedingly desirable and extended lasting materials that can face up to environmental pressures such as ultraviolet radiation, chemicals, and temperature fluctuations.
2. Strength: The membrane pick to have ample tensile electrical electrical energy and tear resistance to successfully stand up to mechanical forces and quit soil erosion. The extensive specifies the minimal electricity requirements for one of a form applications.
![]() |
![]() |
![]() |
![]() |
![]() |
3.Permeability: Geomembranes prefer to have adequate permeability to allow water to omit by at the same time as conserving impenetrable particles. This can make fantastic wonderful drainage and filtration, give up water accumulation, and retain soil stability.
4. Thickness: The favored specifies the minimal and most thickness of geomembranes to make fantastic they furnish the quintessential diploma of security and reinforcement.
5. Durability: The membrane decide on to have a prolonged service existence and hold its integrity and standard common overall performance over time. The elegant specifies sturdiness requirements, which embody tolerance to biodegradation and chemical exposure.
![]() |
![]() |
|
![]() |
![]() |
6. Installation: The well-known affords instructing for the perfect set up techniques, making superb that the geomembrane is hooked up effectually to gather the required performance.
By adhering to these geomembrane standards, we can make tremendous the most exceptional ordinary standard overall performance and agency existence of these materials, imparting reliable and sustainable choices for our clients' projects.
Specifications
|
Properties |
Test Method |
GMSH050 |
GMSH075 |
GMSH100 |
GMSH150 |
GMSH200 |
|
■ Thickness |
ASTM D5199 |
0.50 mm |
0.75 mm |
1.00 mm |
1.50 mm |
2.00 mm |
|
■ Density |
ASTM D1505 |
0.940 g/cc |
0.940 g/cc |
0.940 g/cc |
0.940 g/cc |
0.940 g/cc |
|
Tensile Properties |
|
|
|
|
|
|
|
■ Yield strength ■ Break strength ■ Yield elongation ■ Break elongation |
ASTM D6693 Type IV
|
7 kN/m 13 kN/m 12% 700% |
11 kN/m 20 kN/m 12% 700% |
15 kN/m 27 kN/m 12% 700% |
22 kN/m 40 kN/m 12% 700% |
29 kN/m 53 kN/m 12% 700% |
|
■ Tear Resistance |
ASTM D1004 |
62 N |
93 N |
125 N |
187 N |
249 N |
|
■ Puncture Resistance |
ASTM D4833 |
160 N |
240 N |
320 N |
480 N |
640 N |
|
■ Stress Crack Resistance |
ASTM D5397 |
500 hrs |
500 hrs |
500 hrs |
500 hrs |
500 hrs |
|
■ Carbon Black Content |
ASTM D1603 |
2.0% |
2.0% |
2.0% |
2.0% |
2.0% |
|
■ Carbon Black Dispersion |
ASTM D5596 |
For 10 different views:9 in Categories 1 or 2 and 1 in Category 3 |
||||
|
■ Oxidative Induction Time (OIT) |
ASTM D3895 |
100 min. |
100 min. |
100 min. |
100 min. |
100 min. |
|
■ UV Resistance High Pressure OIT retained after 1600hrs |
ASTM D5885 |
50% |
50% |
50% |
50% |
50% |
|
Dimensions |
|
|
|
|
|
|
|
■ Roll Width (m) |
|
7 |
7 |
7 |
7 |
7 |
|
■ Roll Length (m) |
|
420 |
280 |
210 |
140 |
105 |

Factory strength
![]() |
![]() |
Applications
Applied to the projects of Landfill site, bank, dam, storage reservoir, channel, irrigation, highway, railway, tunnel, drinking tank, salt field bittern pan, chemical liquid storage, treatment tank, artificial lake and riverway etc.

Factory Appearance

RELATED PRODUCTS